- - By stefano.ghidini Date 06-13-2018 12:54
Hallo
I need to know where the acceptance criteria for PT, MT and RT are indicated. I found table 6.1 for VT and 6.2/6.3 for UT
I am preparing a welding table for a new Project and our Client is asking to indicate the acceptance criteria for all the NDE
Thanks
Parent - - By Steelslinger (**) Date 06-13-2018 13:11
What Code?
Parent - - By 803056 (*****) Date 06-13-2018 13:27
Looks like D1.1. Look at clause 6.10.

Al
Parent - By welderbrent (*****) Date 06-13-2018 18:30
What he said...