- - By tinman1954 Date 07-07-2018 15:08
301g trailblazer owners please offer a little help.
I am using my 301g to tig weld and it works fine until the unit reaches full operating temperature (usually about 10 to 15 mins) then there is no welding output. I can shut it off and wait 20 minutes or so then restart it welds fine. No matter how long I leave it off it never welds longer than 15 minutes.
If anyone has experienced this same problem please share your info.
thanks
Parent - - By 522029 (***) Date 07-07-2018 16:50
A known problem is with the gas cap not venting properly. Try running the machine with the cap loose before you try anything else.

HTH
Griff
Parent - By Yaziya Date 07-31-2018 14:42
Thanks for this answer!