- - By MIGUEL TERAN (*) Date 07-19-2018 14:52
Hello all

Is mandatory show the  brand manufacturer to filler metal on PQR and WPS ?? AWS D1.5 Bridge Welding Code

Thank for your advice

Miguel Teran
Parent - - By Steelslinger (**) Date 07-19-2018 19:49
Table 5.2 (D1.5-2015 Edition) specifies the requirement, and Commentary-5.5.1 has a more in depth explanation of the issue.
Parent - By MIGUEL TERAN (*) Date 07-23-2018 06:52
Thank ....I appreciate your information