I am new to fcaw I have my D1.1 l.a city cert manual process and I am working on adding my semi automatic. I am running a NR 232 wire and I just cant seem to get the welds right. Is there anyone who can give me some advice,  a couple of pointers are highly appreciated.

                 Thank you
Parent - By Lawrence (*****) Date 09-17-2018 00:52
Are you welding with the

Polarity?

Current?

Voltage ?

Gun angles ?

That the manufacturer recommends?
Parent - - By Marshallseale82 Date 10-25-2018 21:05
Fluxcore is a force feed process. Can basically weld all positions without any adjustments. But yeah, what they said.
Parent - By 803056 (*****) Date 10-26-2018 19:43
Make sure you set the welding parameters per the manufacturer's recommendations. Don't try to set it by "feel." Pay attention to the electrode extension.