Dear Sir~
According to AWS D1.1, studs may be welded using FCAW, GMAW or SMAW processes.
But, In case of AWS D1.5, studs may be fillet welded by only "SMAW".
Question!!. When AWS D1.5 was applied in project, studs cannot be welded FACW processes?
By
jwright650
Date
10-15-2018 10:58
AWS D1.5 Clause 7.5.5 gives the option to manually weld with SMAW...(no mention of anything else)
By
OWT
Date
10-15-2018 12:17
Thanks sir, then.. Do you know why D1.5 approve only SMAW??
By
jwright650
Date
10-15-2018 21:32
C7.5.5 says the option for manually welded SMAW is if there are a limited number of studs to be welded, you have the option not to use the stud gun. Out in the field, I'm not sure they like FCAW to be used at all.
By
OWT
Date
10-28-2018 23:45
I understand. Thanks.
Topic
AWS.org
/
Forum News & Help
/ Stud welding Process. (D1.1 V.S D1.5)
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill