Hello Everybody.
I need help. Hope somebody can.
I need to weld Super Duplex, (UNS S32750, P No. 10H) to Al-6XN (UNS N08367, P No. 45)
1. Any recommendations for filler Wire?
2. I welding PQR & WPS for the following 10H to P8, 10H to 10H, P45 to P45, P45 to P8, P45 to P43. Can I use any of these to weld P10H to P45??
Appreciate your help. Thank you.