- - By Inspector87 Date 12-17-2018 14:04
I had a disagreement regarding 2.18.1 with my boss and im looking for clarification. I was saying that 2.18.2 is prohibiting flat position bevel grooves when a v groove can practibally be made. Hes saying it say you can if you qualify it. He says it says so in 2.18.1, but 2.18.1 is talking about a completely different prohibited weld. I told him that 2.18.1, 2, 3 and 2.18.4 are all stand alone statements under 2.18 prohibited joints and welds and one does not apply to the other. Is there something I'm missing here?
Parent - - By Steelslinger (**) Date 12-17-2018 17:23
Your reading of it is correct. 2.18.1 has nothing to do with 2.18.2, 2.18.3 or 2.18.4, except they are all Prohibited Joints and Welds.
Parent - By Inspector87 Date 12-17-2018 18:55
Thank you, thats what i thought.
Parent - - By 803056 (*****) Date 12-18-2018 03:27
The clause you cite is applicable to cyclic loads only. So, the particular joint details are not necessarily prohibited, they simply are not permitted if it is possible to use a U-groove or V-groove in a butt joint subject to cyclic loads. They are permitted in other types of joints or where cyclic loading is not an issue.

Al
Parent - By SWN1158 (***) Date 12-18-2018 13:54
Good eye Al !
Parent - By Inspector87 Date 12-20-2018 03:54
Yes i am aware of this, thanks
Parent - By chuckbeardsley Date 01-05-2019 14:03
Thanks