When multi-qualifying a welder to API-1104. If a welder takes both the butt (horizontal) / branch (fixed) tests on 12" (X52), does this qualify him for all grades? If the pipe on the project is X65, is he qualified?
Reason I am asking is 5.4.2.2 C