/ PED 2014/68/EU - Welding procedure qualification
By
Rakhul
Date
01-30-2019 13:01
Hi,
Basic understanding on PED job orders is to mandatory to get qualify welding procedure & welder as per EN ISO 15614-1 / 15609 / 9606
Is this correct?
By
Shane Feder
Date
01-30-2019 23:23
No, you can use ASME welding procedures but additional testing is required to comply with EN ISO 15614-1.
Google PED/ASME/TWI and you will find information explaining this.
Topic
Welding Industry
/
Technical Discussions
/ PED 2014/68/EU - Welding procedure qualification
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill