-Can I use welding Electrode of FCAW ( E71T1) in the Semi automatic welding machine for GMAW ? -The question can be cleared by is the welding machine for GMAW and FCAW may be the same welding machine?
Yes, just be sure to use the correct shielding gas and technique. To figure out what "correct" means, first check the filler metal manufacturer's recommendations, then validate through testing.