Up Topic Welding Industry / General Welding Discussion / Date of Welder qualification as per Asme sec 9
- - By Atuuel (*) Date 03-12-2019 01:27
What is the qualification date of a Welder as per Asme section 9 to fill in Welder certificate. Is it actual date of welding or date of results or date of approval from inspector. Is there any code case or any clause in asme section 9 about this
Parent - - By 803056 (*****) Date 03-12-2019 05:13
The welder isn't qualified until all the testing is completed and someone signs the paperwork.

Al
Parent - By Atuuel (*) Date 03-12-2019 15:10
As per EN ISO 9606-1:
"The validity of the welder’s approval starts from the date of welding of the test piece, provided that the required tests
are satisfactory."

I am searching if any same thing is written in asme section 9 or not.