By newb
Date 03-16-2019 02:52
Edited 03-16-2019 13:03
Hello folks,
I have an assembly that is manufactured from square tubing, wall thickness 0.065" with flare bevel welds. For clarity, the groove weld is at the interface of the bend radius of the tube and an adjoining plate. AWS D1.1-2015 refers to Table 9.11 for qualification of PJP groove welds; however, my tube wall thickness is less than the minimum defined in table. Can someone point me in the right direction?
Thanks in advance.