Gents,
i need information regarding Lack of Fusion acceptance criteria as per AWS D 1.1 (for Welder qualification)
By
jwright650
Date
05-22-2019 16:08
Clause 4.16.1.1, see Clause 4.22.3,
By
803056
Date
05-22-2019 19:08
AWS D1.1 does not use the term "lack of fusion". D1.1 calls it "incomplete fusion".
Al
Topic
AWS.org
/
Forum News & Help
/ AWS D1.1 Acceptance Criteria for Lack of Fusion in RT / UT
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill