Welcome to the forum Prasanta
The major manufacturers have spend 50 years developing their "recipe" for making fluxes. It is probably a very closely guarded secret.
There values given by ASME Section 2 Part C (Edition 2010 - Addenda 2011) :
Also values published by AWS A5.1