Could you help me to make clear the situation?

Our welding procedure qualified on base metal group II, DN200, 12.7 mm, 6GR, Figure 9.25.
Does this WPS apply for all CJP butt welds (pipe & box) without backing one side? or we need to run a new PQR at 6G position to cover butt weld without backing one side?

Thanks