Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Inspection & Qualification / D1.1 Fillet Weld Break & Macroetch test plate - Option 1
- - By dfisher Date 10-14-2019 18:30
Good Afternoon,

I have a question about Figure 4.25 "Fillet Weld Break and Macroetch Test Plate - Welder of Welding Operator Qualification - Option 1" on page 161 of the D1.1M:2015

Is 1/2" plate the only thickness that can be used for Fillet Weld Break qualification, or can other thicknesses (1/4"?) be utilized?

Much appreciated,
Parent - - By SWN1158 (***) Date 10-14-2019 18:46
Notice that Figure 4.25 indicates 1/2 "minimum" thickness on both plates
Parent - By 803056 (*****) Date 10-15-2019 00:19
Nough said.

Al
Up Topic Welding Industry / Inspection & Qualification / D1.1 Fillet Weld Break & Macroetch test plate - Option 1

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill