I am somewhat confused since you refer to both ASME and API in the same sentence.
API 1104 doesn't addressed many of the issues included in AWS structural codes because API doesn't recognize the concept of prequalification. Thus, one must qualify the process, including the techniques, proposed for production to demonstrate the proposed WPS will produce the required mechanical properties.
Al