Dears,
Does the thickness limitation (1.1 x test coupon thickness) for GMAW Short circuit is applicable for Fillet weld procedure qualified with a groove weld test.
By
Jim Hughes
Date
02-24-2020 18:23
No. You are held to 1.1 on base material and thickness qualified but socket welds would be all. You would be good to weld all socket welds.
Topic
Welding Industry
/
ASME Codes
/ GMAW-Short circuit Tranfer mode (ASME SEC IX)
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill