- - By Marc Miller Date 12-12-2019 17:23
Hi everyone,
I work for an oil and gas company in the Houston area and am looking for some companies that do welder qualification. We currently use TUV but are looking for some alternatives. The qualifications would need to cover various pipe and plate procedures on carbon and stainless.
    Thanks,
          Marc
Parent - By Lawrence (*****) Date 12-13-2019 19:23
I’ve dealt with “Maverick” many times and found them always up to the task.
Parent - By Jim Hughes (***) Date 12-23-2019 14:25
There is WTI , ALS Maverick, or Dynamic Testing, all in Deer Park. WTI is the cheapest, for PQ and welder testing.