There are many conversion charts on the internet. The one I found for sheet metal shows....
14 ga conversion for standard steel = 1.897 mm
14 ga conversion for non ferrous/aluminum = 1.628 mm
14 ga conversion for galvanized steel = 1.994 mm
Hopefully this answers your question.