Hi,

We want to weld ss 304 or 316 (non pressure parts) to Gr. 11/22/91. Which is the most suitable SMAW electrode to join these dissimilar welds?
We are currently using 309 or ENiCrFe-3 (depending upon temp.)
Which are other cost effective electrodes instead of this inconel electrode.
Parent - By 803056 (*****) Date 01-28-2020 14:33
The electrode with the least amount of nickel will be the lowest cost.