Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Metallurgy / Possibilities of transvers weld crack
- - By Dhrumil Chauhan Date 09-03-2020 07:02
Dear,

We have observed transverse weld crack in saw welding in API 5L X70M material grade linepipe.
In order to find potential cause for same we have carried out chemical analysis which shows higher amount of Cu content arround > 1%.

During etching we also observed blackness in particular cracked portion during microscopic analysis. More or less no phase changes observed.

Regards,
Dhrumil Chauhan

Email: dhrumilchauhan0@gmail.com
Phone : 8866494026
Parent - By 803056 (*****) Date 09-03-2020 12:44
What electrode and flux did you use?

Al
Up Topic Welding Industry / Metallurgy / Possibilities of transvers weld crack

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill