- - By Steve Parmelee Date 02-05-2021 00:20
Hello all,
Maybe it's because I've spent so much time staring at the book but, I can't seem to find the max. single pass SAW fillet weld when welding A709-50W in the horizontal position. Can anyone help?

Thank you for your time.
Parent - By Jim Hughes (***) Date 02-11-2021 21:18
Steve,
I assume you are speaking about a PQ not welder qual.? Look at 5.23.2.4. It should tell you what you need to know. You have a couple of options detailed in that section.