Ok,For anybody who wanted to build a real simple welding table:

Material:

4- 2x2x3/16 in sq steel tubing-that will be for the legs
1-2ftx2ftx1/4 steel plate-that will be for the top

Simply Arc weld the 4 pieces of tubing to the plate and then if you want you could put some extra attatchments like I did for mine like an electrode holder made out of angle and a shelf on the bottom welded to the legs made also out of angle with some steel mesh and then for mobility so you don't have to carry around this table you could weld you some casters on the bottom of the legs and then if you think the 1/4 inch plate on top is not thick enough then you could tack a 2x2 foot 3/8 inch plate on top.Although I really reccomend Arc Welding You could Use Metal Inert Gas as Well.The table came in real handy for me but I got about 5 different tables of all different kinds but try this one out.
Up Topic Welding Industry / General Welding Discussion / Simple Table Plans

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill