- - By ilkinhasanov (*) Date 07-12-2021 06:13
HI All,

Could you please advise, what are advantages & disadvantages for Using of Super-Duplex Wire for welding of Duplex Material?

Regards,
Ilkin HASANOV
Parent - By Jim Hughes (***) Date 07-19-2021 10:54
Needless over alloying and spending money that you don't need to. That is the simple answer without knowing what the application is that you are wanting to use this metallurgy for. Bill Newell has some great literature on this subject. It's euroweld.com.