Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / General Welding Discussion / Questions about lanthanated tungsten
- - By T0M (*) Date 12-24-2003 23:42
I am looking for a good all around tungsten. I will be doing mostly aluminum but will be doing some steel as well.
I have been reading about lanthanated tungsten, and Am guessing this is the universal tungsten of choice.
My question is which one to get?
1% (black), 1 1/2%(yellow) or 2%(blue)?

whats the difference in performance of these three?

Thanks
Tom
Parent - By T0M (*) Date 12-26-2003 03:43
Also, I have seen lanthanated tungsten real cheap on ebay, is there such a thing as cheap or poor quality tungsten? If so what is a good name to get?