- - By MTG Date 01-28-2004 14:09
Looking to buy a consumable insert ring roller. Does anybody know of a manufacturer to purchase one from.
Thanks,
Mike CWI Virginia
Parent - By MBSims (****) Date 01-31-2004 17:07
This should work:

http://www.toolsplus1.com/basic_ringroller.htm

You may need to have some grooves machined in the rolls for the type of insert you use, but that should not cost much.