- - By jnye Date 02-03-2004 14:31
This question concerns the brazing of SS304 and niobium (w/1% Zr).

I've successfully silver brazed niobium and SS304 together using a 56% silver braze made by safety-silv (J.W. Harris). I would like to know if there are any other options such as the use of copper or nickel brazing alloys. Thanks
Parent - By dee (***) Date 02-03-2004 19:55
jnye,
I am familiar with the Harris product, but not with niobium, and I have a limited number of references and literature with which to help, but I am curious as to what the property you are looking for in the alloy would be... what's wrong with the Safety-Silv?