- - By husain Date 03-04-2004 07:22
WE NEED ER 4043 GRADE ALUMINIUM WIRE FOR TIG WELDING FOR SPECIAL APPLICATION. CAN ANY BODY HELP US TO FIND THE MANUFACTURERS. KINDLY GIVE US THE MANUFACTURERS DETALS AND EMAIL ADDRESSREQUIREMENT IS FOR 1.6MM, 3.2MM DIA EACH 10 KGS INTITALY
REGARDS
REDDY
Parent - - By EVWELDER (**) Date 03-04-2004 13:49
I use ER 4043 the company name is Alcotech wire corp.Their address is 2750 Aero park drive Traverse city,Michigan 49686 USA.E-mail is alcotec@traverse.com.







Hope that helps you.
Parent - By SA-200 (**) Date 03-04-2004 14:05
http://www.lincolnelectric.com/products/ads/miguarantee.asp