- - By alisharif (*) Date 03-21-2004 07:33
Dear sir
I didnt see any clear procedure and chart for PWHT of Cr steel in ASME Code.Do you know any reference or internet site for complete explanation of PWHT?

thanks a lot
A.Sharif
Parent - By MBSims (****) Date 03-21-2004 17:44
The ASME Code is not intended to provide procedures and instructions. Those come from qualified engineering personnel and are part of the quality program required to perform work under the ASME Code.

Here's some info on PWHT:

http://www.jflf.org/pdfs/papers/keyconcepts4.pdf

http://www.nationalboard.net/Classics/classic2.html