I am making some tables out of naval bronze. I am using this alloy since it forges nicely but I must weld it too. The welds are on some heavy sections (1"x2"). They need to look good but will not be subject to a great deal of stress. Does anyone have advice on the best method to use, mig tig oxy acet or stick, and what procedures to follow?
Parent - By dsergison (*) Date 04-15-2004 13:50
if you can make a well fitted joint then consider soldering it.