By -
Date 09-15-2000 15:02
We're in the process of ISO'izng our weld shop. I'm planning to provide process instructions/WPS info through workmanship samples. I can't use these same samples as weld quality boundry samples due to constraints of ISO compliance. Can someone point me to a wall chart or large defect sample board that the welder's can reference for visual inspection? Thanks.