Welding Industry
/
Technical Discussions
/ Continuous weld test of erw pipes
By
ptccal
Date
09-20-2000 10:20
Dear Sir,
Pls tell me the cheapest on line process to check the weld of erw pipes other than eddie current test and ultrasonic test...
thank you
regards
Mukesh Agarwal
By
R. Johnson
Date
09-21-2000 17:19
Eddy current testing is going to be your cheapest method. Especially if you have any great volume to inspect.
By
NDTIII
Date
10-23-2000 13:35
The fastest way would be to have a UT hand scanner with 4 transducers and a multiplexer connected to 4 scopes or a multi-channel scope using water as your couplant and confirm all indications manually.
Topic
Welding Industry
/
Technical Discussions
/ Continuous weld test of erw pipes
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill