I have to weld on a komatsu dozer frame,their procedure says to an electrode that conforms to JIS D4316 or D4326, (on the IFS 1998 disc it does not have a cross refference for this electrode) is there another electrode that can be used or do I have to find some of this?
Parent - By thirdeye (***) Date 07-19-2004 18:51
Metalloy is showing E7016.

http://www.metalloy.co.uk/minicat/it010011.htm

Your consumable supplier should be able to confirm this.
Parent - - By Niekie3 (***) Date 07-20-2004 07:28
Hi

Just to confirm, it is E7016. I believe that E7018 should also do the job.

Regards
Niekie Jooste
Fabristruct Solutions
Parent - By minerwelder Date 07-20-2004 13:41
Thanks for your help I'll go to the job of welding now.