Can a have a welder weld one coupon and have the lab give me two RT reader sheets? One for ASME and the other for AWS. My intent is to get a ASME WPQ and a AWS WPQR from one coupon.
I see no problem with what you purpose. I used to do that many years ago. I believe the only difference is the area of the film that is read for each code.