- - By dlmann (**) Date 08-21-2004 17:41
Does anybody use Code Case 2326 that permits use of ultrasonic examination (UT) of welder test coupons in lieu of radiography (RT)? Where can one get ahold of this code case without buying the entire code case catalog?
Parent - - By thirdeye (***) Date 08-21-2004 20:27
Hi dlmann,

Here is a link to the code case review page. The code cases appear here for a short period of time and can be printed. I did not see 2326 on the list. A couple of months ago I had some questions about 2235 and it was available for review then, but I did not see it on the list now either.

http://cstools.asme.org/wbpms/public/index.cfm?PublicReview=CodeCase

This link is to the proposed code revisions page:
http://cstools.asme.org/wbpms/public/index.cfm?PublicReview=Revisions

This link is to the code case database:
http://cstools.asme.org/CodeCases.cfm

If you stumble onto paydirt, let me know. You don't get much free from ASME.

Parent - By gunung Date 05-14-2005 06:39
Dear Thirdeye,

I'm looking for ASME code case 2476.

Really appreciate if you can email me a copy.

Thx in advance.

shahirah@netvigator.co.uk
Parent - By mraschis (*) Date 05-19-2005 02:54
Dlmann Do you have the ASME Code Case 2235? If yes, Can you send me a copy?

Does anyone have ASME Code Case 2235?
Parent - - By MBSims (****) Date 08-21-2004 20:43
Have you tried calling Global/IHS? Their phone number is 800-854-7179. I checked their website, but they only list the complete volume of Code Cases. If you ask on the phone, they may provide the single code case. I know a single code case can be downloaded separately if you are an IHS subscriber, so they should be willing to sell it separately.
Parent - - By NDTIII (***) Date 08-22-2004 03:13
Provide your email address and I will give you a copy.
Parent - By mraschis (*) Date 05-19-2005 21:51
NDTIII Do you have ASME Code Case 2235?