http://www.jwharris.com/jwref/chart/
scroll down to the bottom to see "aluminum to aluminum". There are melting temps, recommended fluxes/cleaning and typical heat sources that would be needed, shown in this filler selection chart. On the left of the screen are more links to additional info, check that out also.
Hope this helps,
John Wright