When we use E6010 electrode in 2.5 mm diameter, the arc burning is ecentric. This problem is not observed in larger dia electrodes and when this 2.5mm electrode is used for root pass. the problem only appears when using this dia for hot passes.
Any comments and advice?
Thanks