Michael,
Have you considered AWS D1.6- Stainless Welding Code. I qualified a pWPS for a company recently covering spary transfer, short arc and pulse arc. These all were within the pre-qualified essential variables and performed quite well. The joint design was B-U2-GF.
John Folk