Anyone have any experience with weld studs?
I was thinking of using them as part of a bracket, and I thought I'd see if there were any issues welding them. (Ref. McMaster Carr pg 3013 & 3061). Will Zinc plated steel weld well to carbon steel sheetmetal (which later gets painted, thats why the stud need to be plated - or maybe stainless???) ?
Pete