I have a pressure vessel weld overlayed inside by Inconel 625 .now I have founded some area has un bonded to CS layer.
Client spec requires to remove and repair it, but it does not specify how much is acceptance criteria .
Does any body know applicable standard reference of acceptance criteria for unbonded clad?
Thanks in advnce for responces.