- - By BIG E (*) Date 01-15-2005 19:37
Ok I switched from the standard #10 green to gold # 10 and befor I went to strike a arc I am always in the habit of inspecting my equiptment. Found what looked like a wave of discoloration on my gold lens brand new never used it looks like a rainbow oil sheen but in the filter itself should I toss it? or is it ok?
Parent - - By harleyhitman (**) Date 01-16-2005 04:48
I wouldn't use it, sounds like it is damaged
Parent - By n5uzt (**) Date 01-16-2005 16:38
if any of the gold coating is gone do not use