Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic American Welding Society Services / Certifications / ROBOT welding
- By n5uzt (**) Date 01-29-2005 01:37
any one have any experence doing wps and woqr for robot stations
what tests do you do and what paper work do you use?
same as a manual welder?
robots welding on mild steel 26ga to 10ga. flat posit.
mig welding solid e70s-3 and 70s-6
ar/co2 92/8 spray mode.
do prequailfied wps apply?
multiple stations doing the same work one set of papers
enough for each station? i guess each operator would have to be tested as well as the robot it self?