By -
Date 02-04-2005 07:09
Hello
I need a test plate for the material mention above.
The chemical composition are: C=0,26, Mn=0,97 Ce=0,47
Yield Strength (PSI x 100) 447, Tensile Strength 791
The size have to be Gauge 10" x Width 10" x Length 10"
We have our factory in Norway.