Hi I would suggest looking at the FV520B type composition ie 14Cr,5Ni,1.5Mo. This also has Cu and a wiff of Nb (Cb) and is a precipitation hardening martensitic SS. This is commercially available go to www.metrode.com if this meets your requirements?