We are preparing to weld some Nickel pipe Alloy 200. The puddle just does not want to flow, by nature. Does anyone have any suggestions to help? Any and all welcomed.
See the reply in the Technical Section of this forum. Use the 'dip" method or the "key hole" method and work the metal with your tungsten. Nickel has very bad fluidity.