- - By klt Date 07-29-2005 01:59
I am very new to the welding industry. Anyway, I have a problem that one of our contractor requests me to confirm the use of AWS A5.20-95, E70T-4 with AWS A5.29-98, E70T-K2 as an alternate. Why does he want to do that?
Please help.
Ken Lumpard
kenlumpard@cox.net
Parent - By swnorris (****) Date 07-29-2005 12:36
I can't understand the E70T-4, because it has a low sensitivity to cracking. E70T-K2 has 1.5% nickel for more notch toughness.