- - By GlynnT Date 08-26-2005 13:26
I have a drawing for an inconel 718 component that has a dowel pin welded into it using ASM51G filler material. I haven't been able to find anything remotely like that on the net and was hoping someone here may be able to enlighten me.

All the best,

Glynn.
Parent - By SWP (**) Date 08-26-2005 14:24
You might ask http://www.usweldingcorp.com/main.htm, they deal with a lot of "aerospace" alloys.
Also http://www.haynesintl.com/, manufactures alloys such as IN-718.
Parent - By Bill Mc (**) Date 08-29-2005 17:18
Special Metals inc. has a filler metal called "INCONEL Filler Metal 718" It is a solid wire. It complied with AWS /SFA 5.14, class ERNiFeCr-2.

Link to a vendor:
http://www.specialmetalswelding.com/products/mig/mig.htm