/ welding cast alum. wheel?
By
lazy_lidz
Date
10-30-2005 23:51
heres the problem, i am trying to fill in and smooth some lettering on the spoke of a 15 inch cast alum. rim useing GTAW. i was wondering what rod to use? size? alloy?
By
srw2506
Date
11-14-2005 20:23
Depending on the ride you want,dont weld on rims,its dangerous it will throw them out of balance and its just foolish,buy new rims.
Topic
American Welding Society Services
/
Technical Standards & Publications
/ welding cast alum. wheel?
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill