- - By nimajavidan (*) Date 03-14-2006 10:59
Dear Friends,
does a Short circuit GMAW process need to qualified or prequalified procedures include S.C mig/mag process?
which standard state that?
Thank you in advance
Nima
Parent - By jwright650 (*****) Date 03-14-2006 12:33
I replied to your other thread in "Technical".
John Wright
Parent - By brande (***) Date 04-23-2006 04:32
Short circuit is never prequalified under AWS code.

All short circuit (short arc) must be qualified.


Good Luck